Microscopic examination of the fracture surfaces of a cold working die due to premature failure D Statharas, J Sideris, C Medrea, I Chicinaş Engineering Failure Analysis 18 (2), 759-765, 2011 | 21 | 2011 |
Getting the strain under control: Trans-Varestraint tests for hot cracking susceptibility D Statharas, H Atkinson, ROB Thornton, J Marsden, H Dong, S Wen Metallurgical and Materials Transactions A 50, 1748-1762, 2019 | 18 | 2019 |
Preliminary examination of the fracture surfaces of a cold working die D Statharas, D Papageorgiou, J Sideris, C Medrea International Journal of Material Forming 1 (Suppl 1), 431-434, 2008 | 12 | 2008 |
Nanocomposite Co-nSiC coatings electrodeposited from cobalt-gluconate bath via pulse reverse plating technique with anionic surfactant DP Weston, D Albusalih, H Hilton-Tapp, D Statharas, SP Gill, J Navajas, ... Materials Chemistry and Physics 305, 127943, 2023 | 4 | 2023 |
THE ROLE OF THE DESIGN IN PREVENTION OF TOOL STEEL FAILURES. CASES OF STUDY C Medrea, J Sideris, D Papageorgiou, D Statharas INTED2009 Proceedings, 4080-4088, 2009 | 2 | 2009 |
Development of Multilayer Coating Systems for Self-Healing Protection And Corrosion Mitigation in the Atmospheric Zone of Offshore Wind Turbines. A Loukodimou, D Weston, D Statharas, S Paul AMPP CORROSION, D051S056R009, 2022 | | 2022 |
Experimental Characterization Of API-5L X65 Steel And An Improved, Reliable Method For Assessing Hot Cracking Susceptibility Of Materials D Statharas University of Leicester, 2019 | | 2019 |
Failure analysis of two cold-working cutting tools. Case studies C Medrea, L Fragkos-Livanios, KI Giannakopoulos, D Statharas MATEC Web of Conferences 188, 04026, 2018 | | 2018 |
PRELIMINARY EXAMINATION OF THE FRACTURE SURFACES OF A COLD CUTTING TOOL D Statharas, J Sideris, D Papageorgiou, C Medrea INTED2009 Proceedings, 4101-4106, 2009 | | 2009 |