Structural, microstructural and impedance spectroscopy study of functional ferroelectric ceramic materials based on barium titanate
B Garbarz-Glos, W Bak, M Antonova, M Pawlik
IOP Conference Series: Materials Science and Engineering 49 (1), 012031, 2013
382013
Effect of Axial Pressure on Electric Properties of Pb‐Modified Na0.5Bi0.5Tio3 Ceramic
J Suchanicz, JP Mercurio, S Said, B Garbarz‐Glos
physica status solidi (a) 193 (1), 179-186, 2002
312002
Effect of Zr4+ doping on the electrical properties of BaTiO3 ceramics
B Garbarz-Glos, K Bormanis, D Sitko
Ferroelectrics 417 (1), 118-123, 2011
282011
Low temperature measurements by infrared spectroscopy in CoFe2O4 ceramic
R Bujakiewicz-Korońska, Ł Hetmańczyk, B Garbarz-Glos, A Budziak, ...
Open Physics 10 (5), 1137-1143, 2012
262012
PLZT—Synthesis, sintering and ceramics microstructure
M Dambekalne, M Antonova, M Livinsh, B Garbarz-Glos, W Smiga, ...
Journal of the European Ceramic Society 26 (14), 2963-2966, 2006
262006
Dielectric properties of BaTiO3 based materials with addition of transition metal ions with variable valence
D Sitko, W Bak, B Garbarz-Glos, A Budziak, C Kajtoch, A Kalvane
IOP Conference Series: Materials Science and Engineering 49 (1), 012050, 2013
152013
Microstructure, calorimetric and dielectric investigation of hafnium doped barium titanate ceramics
B Garbarz-Glos, W Bąk, A Molak, A Kalvane
Phase Transitions 86 (9), 917-925, 2013
152013
The electrical properties of Ba1-ySryZrxTi1-xO3 solid solution
B Garbarz-Glos, D Sitko, A Budziak, K Bormanis, M Antonova, ...
Ferroelectrics 424 (1), 36-41, 2011
152011
Structural and mechanical properties of ceramic solid solutions Na1-xLixNbO3 for x≤ 0.06
W Śmiga, B Garbarz-Glos
Ferroelectrics 377 (1), 137-145, 2008
152008
Dielectric properties of SbSI-modifed in phase transition region
B Garbarz-Glos
Ferroelectrics 292 (1), 137-143, 2003
152003
Electrical Properties of Na 0.98 Li 0.02 NbO 3 Under Axial Pressure in Phase Transition Region
W Smiga, B Garbarz-Glos, C Kuś, J Suchanicz, M Burzyńska
Ferroelectrics 292 (1), 145-150, 2003
142003
Ultrasonication as a method of investigation of the mechanical properties of doped hafnium barium titanate
B Garbarz-Glos, W Piekarczyk, I Smeltere, W Śmiga, M Antonova
Ferroelectrics 436 (1), 87-95, 2012
132012
Structural, thermal expansion and heat capacity study of lead-free [(1 − x)(Na0.5Bi0.5)–xBa]Zr1−y Ti y O3 ceramics
J Suchanicz, G Stopa, J Kusz, M Zubko, W Hofmeister, M Antonova, ...
Journal of materials science 45, 1453-1458, 2010
132010
Evaluation of Rhodamine B Photocatalytic Degradation over BaTiO3-MnO2 Ceramic Materials
I Kuźniarska-Biernacka, B Garbarz-Glos, E Skiba, W Maniukiewicz, W Bąk, ...
Materials 14 (12), 3152, 2021
122021
The effects of the additive of Eu ions on elastic and electric properties of BaTiO3 ceramics
D Sitko, B Garbarz-Glos, W Piekarczyk, W Śmiga, M Antonova
Integrated Ferroelectrics 173 (1), 31-37, 2016
112016
Dielectric and ferroelectric properties of lead-free NKN and NKN-based ceramics
J Suchanicz, I Smeltere, A Finder, K Konieczny, B Garbarz-Glos, ...
Ferroelectrics 424 (1), 53-58, 2011
112011
Electrical characterization of the Fe-doped BT ceramics by an impedance spectroscopy
D Sitko, B Garbarz-Glos, M Livinsh, W Bąk, M Antonova, C Kajtoch
Ferroelectrics 486 (1), 8-12, 2015
102015
Elastic properties of barium zirconate titanate ceramics
B Garbarz-Glos, K Bormanis, A Kalvane, I Jankowska-Sumara, A Budziak, ...
Integrated Ferroelectrics 123 (1), 130-136, 2011
92011
Dielectric Properties of Na0.5K0.5(Nb1-xSbx)O3+MnO2 Ceramics (x = 0.04, 0.05 and 0.06)
J Suchanicz, A Finder, I Smeltere, K Konieczny, I Jankowska-Sumara, ...
Integrated Ferroelectrics 123 (1), 102-107, 2011
92011
DIFFERENTIAL SCANNING CALORIMETRY INVESTIGATION OF PHASE TRANSITION IN BaZrXTi1-XO3
B Garbarz-Glos, R Bujakiewicz-Korońska, D Majda, M Antonova, ...
Integrated Ferroelectrics 108 (1), 106-115, 2009
92009